Elastomer | ||||
Ethylene-Propylene (EPDM) | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 0.86 *10³ | kg/m³ | 53.7 | lb/ft³ |
---|---|---|---|---|
Tensile strength | 20 | MPa | 2900 | psi |
Elongation | 300 | % | 300 | % |
Glass transition temperature | -75 | ºC | -103 | ºF |
Maximum work temperature | 100 | ºC | 212 | ºF |
Electric resistivity | 108 | Ohm*m | 1010 | |
Dielectric constant | 3.3 | - | 3.3 | - |
Applications: electrical insulation, shoe soles, hoses, conveyor belts.