Thermoplastic elastomer Styrene-Butadiene

(submitted by the website administration)

Thermoplastic Elastomer
Styrene-Butadiene
Property Value in metric unit Value in US unit
Density 0.99*10³ kg/m³ 61.8 lb/ft³
Tensile strength 14 MPa 2030 psi
Elongation 700 % 700 %
Maximum work temperature 80 ºC 176 ºF
  • Excellent impact resistance;
  • Good abrasion resistance;
  • Poor resistance to oil, fuel, solvents.

Applications: food packaging, conveyor belts, disposable medical products, wire and cable isolation, tires, shoe soles