| Elastomer | ||||
| Thermoplastic Polyurethane | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.18 *10³ | kg/m³ | 73.7 | lb/ft³ |
|---|---|---|---|---|
| Tensile strength | 40 | MPa | 5800 | psi |
| Elongation | 650 | % | 650 | % |
| Glass transition temperature | -60 | ºC | -76 | ºF |
| Maximum work temperature | 80 | ºC | 176 | ºF |
| Electric resistivity | 104 | Ohm*m | 106 | Ohm*cm |
| Dielectric constant | 6 | - | 6 | - |
Applications: foam elastic parts, bumpers, cable jackets, solid tires, chute linings, gaskets, diaphragms, shaft couplings.