SubsTech     
SubsTech     

to Elastomers
to Properties of polymers

Elastomer Polyisoprene (natural rubber)

(submitted by the website administration)

Elastomer
Polyisoprene (natural rubber)
Property Value in metric unit Value in US unit
Density 0.93 *10³ kg/m³ 58.1 lb/ft³
Tensile strength 20 MPa 2900 psi
Elongation 800 % 800 %
Glass transition temperature -70 ºC -94 ºF
Maximum work temperature 80 ºC 176 ºF
Electric resistivity 107-109 Ohm*m 109-1011 Ohm*cm
Dielectric constant 2.7 - 2.7 -
  • Excellent abrasion resistance;
  • Excellent tear strength;
  • Excellent resilinence;
  • Excellent low temperature flexibility;
  • Excellent dielectric strength;
  • Poor resistance to ozone and oxygen;
  • Poor resistance to sunlight and heat;
  • Poor resistance to solvents.

Applications: automobile tires, gaskets, hoses.

Related internal links

elastomer_polyisoprene_natural_rubber.txt · Last modified: 2023/12/14 by dmitri_kopeliovich