to
Materials Data
to
Metals
Properties of copper alloys
Properties of wrought copper alloys
Wrought copper C10100 (Oxygen-Free Electronic Copper)
Wrought copper alloy C15000 (Zirconium Copper)
Wrought copper alloy C17000 (Beryllium Copper)
Wrought copper alloy C18200 (Chromium Copper)
Wrought copper alloy C24000 (Low Brass)
Wrought copper alloy C26000 (Cartridge Brass)
Wrought copper alloy C27000 (Yellow Brass)
Wrought copper alloy C28000 (Muntz Metal)
Wrought copper alloy C35000 (Medium Leaded Brass)
Wrought copper alloy C36000 (Free-Cutting Brass)
Wrought copper alloy C43500 (Tin Brass)
Wrought copper alloy C46400 (Uninhibited Naval Brass)
Wrought copper alloy C50500 (Phosphor Bronze 1.25% E)
Wrought copper alloy C51000 (Phosphor Bronze 5% A)
Wrought copper alloy C52100 (Phosphor Bronze 8% C)
Wrought copper alloy C52400 (Phosphor Bronze 10% D)
Wrought copper alloy C54400 (Lead Phosphor Bronze B-2)
Wrought copper alloy C61000 (Aluminum Bronze)
Wrought copper alloy C61400 (Aluminum Bronze)
Wrought copper alloy C62300 (Aluminum Bronze)
Wrought copper alloy C63000 (Aluminum Bronze)
Wrought copper alloy C64200 (Aluminum Bronze)
Wrought copper alloy C65100 (Low-silicon Bronze B)
Wrought copper alloy C65400 (Silicon Bronze)
Wrought copper alloy C65500 (High-silicon Bronze A)
Wrought copper alloy C70400 (Copper-Nickel 5%)
Wrought copper alloy C70600 (Copper-Nickel 10%)
Wrought copper alloy C71000 (Copper-Nickel 20%)
Wrought copper alloy C71500 (Copper-Nickel 30%)
Wrought copper alloy C74500 (Nickel Silver 65-10)
Wrought copper alloy C75200 (Nickel Silver 65-18)
Wrought copper alloy C75400 (Nickel Silver 65-15)
Wrought copper alloy C75700 (Nickel Silver 65-12)
Wrought copper alloy C77000 (Nickel Silver 55-18)
Wrought copper alloy C72900 (Spinodal Bronze ToughMet3 AT)
Wrought copper alloy C72900 (Spinodal Bronze ToughMet3 TS)
Properties of cast copper alloys
Cast copper C80100 (Copper)
Cast copper C80410 (Copper)
Cast copper alloy C81500 (Chromium Copper)
Cast copper alloy C82700 (Beryllium Copper)
Cast copper alloy C83600 (Ounce Metal)
Cast copper alloy C84400 (Valve Metal)
Cast copper alloy C84800 (Plumbing Goods Brass)
Cast copper alloy C85200 (Leaded Yellow Brass)
Cast copper alloy C85400 (No.1 Yellow Brass)
Cast copper alloy C85500 (Yellow Brass)
Cast copper alloy C86100 (Manganese Bronze)
Cast copper alloy C86200 (Manganese Bronze)
Cast copper alloy C86500 (Manganese Bronze)
Cast copper alloy C86700 (Manganese Bronze)
Cast copper alloy C87400 (Silicon Bronze/Silicon Brass)
Cast copper alloy C87500 (Silicon Bronze/Silicon Brass)
Cast copper alloy C87600 (Silicon Bronze/Silicon Brass)
Cast copper alloy C87850 (Silicon Bronze/Silicon Brass)
Cast copper alloy C90300 (Tin Bronze)
Cast copper alloy C90500 (Gun Metal)
Cast copper alloy C90700 (Tin Bronze, 65)
Cast copper alloy C91700 (Nickel Gear Bronze)
Cast copper alloy C92200 (Naval M Bronze)
Cast copper alloy C92700 (Leaded Tin Bronze)
Cast copper alloy C93700 (Bearing Bronze)
Cast copper alloy C93800 (Anti-Acid Metal)
Cast copper alloy C94300 (Soft Bronze)
Cast copper alloy C95200 (Aluminum Bronze)
Cast copper alloy C95500 (Aluminum Bronze)
Cast copper alloy C95600 (Aluminum Bronze)
Cast copper alloy C95700 (Aluminum Bronze)
Cast copper alloy C95800 (Aluminum Bronze)
Cast copper alloy C96300 (Copper-Nickel)
Cast copper alloy C96400 (70-30 Copper-Nickel)
Cast copper alloy C97300 (Nickel-Silver 12% Ni)
Cast copper alloy C97600 (Nickel-Silver 20% Ni)
Cast copper alloy C97800 (Nickel-Silver 25% Ni)
Spinodal Bronze Nicomet
Cast copper alloy C96970 (Spinodal Bronze ToughMet2 CX)
Cast copper alloy C96900 (Spinodal Bronze ToughMet3 CX)
Cast copper special alloy C99300 (Incramet 800)
Cast copper special alloy C99400 (Non-Dezincification Alloy)
Cast copper special alloy C99700 (White Manganese Brass)
Cast copper special alloy C99750
Related internal links
Properties of steels and cast irons
Properties of aluminum alloys
Properties of magnesium alloys
Properties of nickel alloys
Properties of gold alloys
Properties of silver alloys
Properties of platinum alloys
Properties of titanium alloys
Properties of ceramics
Properties of carbon materials
Properties of polymers
Properties of composites
Properties of fluids
Copper alloys
to
Materials Data
to
Metals