Cast copper alloy C85500 (Yellow Brass) | ||||
Chemical composition: Zn=41.0%, Cu=69% | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 8.41 *10³ | kg/m³ | 525 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 103 | GPa | 15000 | ksi |
Thermal expansion (20 ºC) | 21.2*10-6 | ºCˉ¹ | 11.8*10-6 | in/(in* ºF) |
Specific heat capacity | 377 | J/(kg*K) | 0.090 | BTU/(lb*ºF) |
Thermal conductivity | 116 | W/(m*K) | 804 | BTU*in/(hr*ft²*ºF) |
Electric resistivity | 6.6*10-8 | Ohm*m | 6.6*10-6 | Ohm*cm |
Tensile strength (sand cast) | 414 | MPa | 60000 | psi |
Yield strength (sand cast) | 159 | MPa | 23000 | psi |
Elongation (sand cast) | 40 | % | 40 | % |
Hardness (sand cast) | 55 | RB | 55 | RB |
Tensile strength (perm. mold) | 371 | MPa | 54000 | psi |
Yield strength (perm. mold) | 160 | MPa | 23000 | psi |
Elongation (permanent mold) | 34 | % | 34 | % |
Hardness (permanent mold) | 53 | RB | 53 | RB |
Liquidus temperature | 900 | ºC | 1652 | ºF |
Solidus temperature | 890 | ºC | 1634 | ºF |