UV cure thixotropic urethane adhesive

(submitted by the website administration)

UV cure thixotropic urethane adhesive
UV cure thixotropic single component electrically insulating urethane adhesive
Property Value in metric unit Value in US unit
Density 1.02 *10³ kg/m³ 68.7 lb/ft³
Viscosity thixotropic paste
Hardness, Durometer A 80 A 80 A
Solids 100 % 100 %
Glass transition temperature -60 ºC -76 ºF
Thermal expansion (20 ºC) 2.4*10-4 ºCˉ¹ 1.3*10-4 in/(in* ºF)
Volume resistivity 5.4*1014 ohm*cm 2.1*1014 ohm*in
Dielectric strength, 0.003” film > 60 KV/mm > 1500 V/mil
Dielectric constant (1kHz) 3.5 3.5
Dissipation factor (1kHz) 0.03 0.03
Insulation resistance 1*1013 ohm 1*1013 ohm