Polyvinyl acetate adhesive
High viscosity homopolymer aqueous emulsion of vinyl acetate stabilised with polyvinyl alcohol
Property Value in metric unit Value in US unit
Density 1.10 *10³ kg/m³ 68.7 lb/ft³
Viscosity at 77°F (25°C) 15000 cP 0.313 lbf*sec/ft²
PH 3 3
Particle size 0.5-3 mkm 2-12*10-5 in
Solids 50 % 50 %
Min. bonding temperature 2 ºC 36 ºF
Service temperature range 5-30 ºC 41-86 ºF