to Elastomers
to Properties of polymers

Thermoplastic elastomer Polyurethane

(submitted by the website administration)

Elastomer
Thermoplastic Polyurethane
Property Value in metric unit Value in US unit
Density 1.18 *10³ kg/m³ 73.7 lb/ft³
Tensile strength 40 MPa 5800 psi
Elongation 650 % 650 %
Glass transition temperature -60 ºC -76 ºF
Maximum work temperature 80 ºC 176 ºF
Electric resistivity 104 Ohm*m 106 Ohm*cm
Dielectric constant 6 - 6 -

Applications: foam elastic parts, bumpers, cable jackets, solid tires, chute linings, gaskets, diaphragms, shaft couplings.