Two component toughened epoxy adhesive | ||||
Two component toughened, thixotropic paste, high strength, high thermal resistance epoxy adhesive | ||||
Property | Value in metric unit | Value in US unit | ||
Viscosity (mixed) at 77°F (25°C) | 300000 | cP | 6.27 | lbf*sec/ft² |
---|---|---|---|---|
Working strength time | 2 | hrs | 2 | hrs |
Full cure time | 72 | hrs | 72 | hrs |
Maximum gap | 5 | mm | 0.2 | in |
Shear strength, steel-to-steel 77°F (25°C) | 16 | MPa | 2320 | psi |
Peel strength, steel-to-steel 77°F (25°C) | 80 | N/(25mm width) | 17 | PIW (lbf/inch width) |
Min. service temperature | -40 | ºC | -40 | ºF |
Max. service temperature | 120 | ºC | 248 | ºF |