Synthetic way lubricant ISO 100 | ||||
Synthetic oil based | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 0.883 *10³ | kg/m³ | 55.1 | lb/ft³ |
---|---|---|---|---|
Kinematic viscosity at 104°F (40°C) | 100 | cSt | 100 | cSt |
Kinematic viscosity at 212°F (100°C)/) | 11.1 | cSt | 11.1 | cSt |
Viscosity index | 95 | 95 | ||
Flash point | 188 | ºC | 370 | ºF |