Way lubricant ISO 150
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.892 *10³ kg/m³ 55.7 lb/ft³
Kinematic viscosity at 104°F (40°C) 143.3 cSt 143.3 cSt
Kinematic viscosity at 212°F (100°C)/) 14.4 cSt 14.4 cSt
Viscosity index 98 98
Flash point 240 ºC 464 ºF
Pour Point -12 ºC -10 ºF
Total acid No. 1.22 1.22
Color 4.5 4.5