Single component high strength, free flowing epoxy adhesive
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 200000 cP 4.18 lbf*sec/ft²
Cure time at 248°F (120°C) 60 min 60 min
Maximum gap 0.5 mm 0.02 in
Shear strength, steel-to-steel 77°F (25°C) 34 MPa 5000 psi
Peel strength, steel-to-steel 77°F (25°C) 112 N/(25mm width) 25 PIW (lbf/inch width)
Min. service temperature -40 ºC -40 ºF
Max. service temperature 180 ºC 355 ºF