Non-heat-treatable Nickel-Chromium-Iron Alloy Inconel 625
Chemical composition: Cr=21.5%, Fe=8%, Mo=9%, Nb=3.65%, Ni=58% min.
Property Value in metric unit Value in US unit
Density 8.44 *10³ kg/m³ 527 lb/ft³
Modulus of elasticity 201 GPa 29200 ksi
Thermal expansion (20 ºC) 12.8*10-6 ºCˉ¹ 7.1*10-6 in/(in* ºF)
Specific heat capacity 410 J/(kg*K) 0.098 BTU/(lb*ºF)
Thermal conductivity 9.8 W/(m*K) 68 BTU*in/(hr*ft²*ºF)
Electric resistivity 129*10-8 Ohm*m 129*10-6 Ohm*cm
Tensile strength (annealed) 800 MPa 128000 psi
Yield strength (annealed) 460 MPa 66700 psi
Elongation (annealed) 50 % 50 %
Liquidus temperature 1350 ºC 2460 ºF
Solidus temperature 1290 ºC 2350 ºF