Non-heat-treatable Nickel-Chromium-Iron Alloy Incoloy 800HT
Chemical composition: Cr=21%, Fe=39.5% min, Al=0.4%, Ti=0.4%, C=0.06%, Ni=32.5%
Property Value in metric unit Value in US unit
Density 7.94*10³ kg/m³ 496 lb/ft³
Modulus of elasticity 196 GPa 28500 ksi
Thermal expansion (20 ºC) 14.4*10-6 ºCˉ¹ 8.0*10-6 in/(in* ºF)
Specific heat capacity 460 J/(kg*K) 0.11 BTU/(lb*ºF)
Thermal conductivity 11.5 W/(m*K) 80 BTU*in/(hr*ft²*ºF)
Electric resistivity 98.9*10-8 Ohm*m 98.9*10-6 Ohm*cm
Tensile strength (annealed) 560 MPa 81200 psi
Yield strength (annealed) 250 MPa 36300 psi
Elongation (annealed) 45 % 45 %
Liquidus temperature 1385 ºC 2525 ºF
Solidus temperature 1357 ºC 2475 ºF