Non-heat-treatable Nickel-Chromium-Iron Alloy Hastelloy X
Chemical composition: Cr=22%, Fe=18%, Mo=9%, W=0.6%, Co=1.5%, C=0.1%, Ni=47%
Property Value in metric unit Value in US unit
Density 8.22*10³ kg/m³ 513 lb/ft³
Modulus of elasticity 196 GPa 28500 ksi
Thermal expansion (20 ºC) 15.5*10-6 ºCˉ¹ 8.3*10-6 in/(in* ºF)
Tensile strength (annealed) 765 MPa 111000 psi
Yield strength (annealed) 380 MPa 55100 psi
Elongation (annealed) 44 % 44 %
Liquidus temperature 1355 ºC 2470 ºF
Solidus temperature 1260 ºC 2300 ºF