High strength anaerobic adhesive
Single component acrylic based adhesive
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 1800 cP 0.0376 lbf*sec/ft²
Fixture time, steel, 77°F (25°C) 10 min 10 min
Maximum gap 0.203 mm 0.008 in
Shear strength, steel, 77°F (25°C) 17 MPa 2465 psi
Min. service temperature -54 ºC -65 ºF
Max. service temperature 150 ºC 302 ºF