Single component acrylic based adhesive
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 1300 cP 0.0272 lbf*sec/ft²
Fixture time, steel, 77°F (25°C) 10 min 10 min
Maximum gap 0.152 mm 0.006 in
Shear strength, steel, 77°F (25°C) 10 MPa 1450 psi
Min. service temperature -54 ºC -65 ºF
Max. service temperature 150 ºC 302 ºF