| Toughened acrylic adhesive | ||||
| Two component (with initiator), toughened, high impact, high thermal resistance acrylic adhesive | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity at 77°F (25°C) | 17000 | cP | 0.355 | lbf*sec/ft² |
|---|---|---|---|---|
| Fixture time | 2 | min | 2 | min |
| Full cure time | 24 | hrs | 24 | hrs |
| Maximum gap | 0.5 | mm | 0.02 | in |
| Shear strength, steel-to-steel 77°F (25°C) | 20 | MPa | 2900 | psi |
| Peel strength, steel-to-steel 77°F (25°C) | 55 | N/(25mm width) | 12 | PIW (lbf/inch width) |
| Min. service temperature | -54 | ºC | -65 | ºF |
| Max. service temperature | 150 | ºC | 302 | ºF |