to Thermosets
to Properties of polymers

Thermoset Phenolics (PF)

(submitted by the website administration)

Thermoset
Phenolics (PF)
Property Value in metric unit Value in US unit
Density 1.40 *10³ kg/m³ 87.4 lb/ft³
Modulus of elasticity (flexural) 8.3 GPa 1200 ksi
Tensile strength 50 MPa 7000 psi
Elongation 1 % 1 %
Flexural strength 69 MPa 10000 psi
Thermal expansion (20 ºC) 40*10-6 ºCˉ¹ 22*10-6 in/(in* ºF)
Maximum work temperature 120 ºC 250 ºF

Applications: wiring devices, lamps holders, switchboards, bottle caps, automotive parts, plugs and switches, handles on kitchen utensils (filled with mineral fibers), motor housings, welding tongs, ashtrays.