SubsTech     
SubsTech     

to Thermosets
to Properties of polymers

Thermoset Unsaturated Polyester (UP)

(submitted by the website administration)

Thermoset
Unsaturated Polyester (UP)
Property Value in metric unit Value in US unit
Density 1.12 *10³ kg/m³ 70.0 lb/ft³
Modulus of elasticity 3.4 GPa 493 ksi
Tensile strength 60 MPa 8700 psi
Elongation 2 % 2 %
Flexural yield strength 113 MPa 16400 psi
Thermal expansion (20 ºC) 31*10-6 ºCˉ¹ 17*10-6 in/(in* ºF)
Thermal conductivity 0.17 W/(m*K) 1.18 BTU*in/(hr*ft²*ºF)
Maximum work temperature 170 ºC 325 ºF
  • Excellent rigidity;
  • High strength;
  • High creep strength;
  • Excellent dielectrical properties;
  • Good chemical resistance;

Applications: fiberglass boats, building panels, fans, fences, helmets, compressor housing, auto body components, bathroom accessories.