General purpose cyanoacrylate adhesive
Single component moisture activated curing adhesives
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 40 cP 8.35*10-4 lbf*sec/ft²
Fixture time, steel, 77°F (25°C) 10 min 10 min
Maximum gap 0.102 mm 0.004 in
Shear strength, steel, 77°F (25°C) 20 MPa 2900 psi
Min. service temperature -54 ºC -65 ºF
Max. service temperature 180 ºC 82 ºF