| General purpose anaerobic adhesive | ||||
| Single component acrylic based adhesive | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity at 77°F (25°C) | 1300 | cP | 0.0272 | lbf*sec/ft² |
|---|---|---|---|---|
| Fixture time, steel, 77°F (25°C) | 10 | min | 10 | min |
| Maximum gap | 0.152 | mm | 0.006 | in |
| Shear strength, steel, 77°F (25°C) | 10 | MPa | 1450 | psi |
| Min. service temperature | -54 | ºC | -65 | ºF |
| Max. service temperature | 150 | ºC | 302 | ºF |