Fast curing cyanoacrylate adhesive

(submitted by the website administration)

Fast curing cyanoacrylate adhesive
Single component moisture activated curing cyanoacrylate adhesives
Property Value in metric unit Value in US unit
Viscosity at 77°F (25°C) 2 cP 4.18*10-5 lbf*sec/ft²
Fixture time, steel, 77°F (25°C) 3 min 3 min
Maximum gap 0.051 mm 0.002 in
Shear strength, steel, 77°F (25°C) 20 MPa 2900 psi
Min. service temperature -54 ºC -65 ºF
Max. service temperature 180 ºC 82 ºF

Related internal links