| Property | Value in metric unit | Value in US unit | ||
| Density | 1.69*10³ | kg/m³ | 105.4 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 1.65 | GPa | 240 | ksi |
| Flexural Modulus | 1.69 | GPa | 245 | ksi |
| Tensile strength | 52 | MPa | 7600 | psi |
| Elongation (max.) | 250 | % | 250 | % |
| Hardness | 80 | Shore D | 80 | Shore D |
| Thermal expansion (20 ºC) | 101*10-6 | ºCˉ¹ | 56*10-6 | in/(in* ºF) |
| Thermal conductivity | 0.15 | W/(m*K) | 1.04 | BTU*in/(hr*ft²*ºF) |
| Melting point | 240 | ºC | 464 | ºF |
| Maximum work temperature | 150 | ºC | 300 | ºF |
| Dielectric constant | 2.5 | - | 2.5 | - |
| Dielectric strength | 79 | kV/mm | 2000 | V/mil |
| Electrical resistivity | >1014 | Ohm*m | >1016 | Ohm*cm |