SubsTech     
SubsTech     

to Thermoplastics
to Properties of polymers

Ethylene tetrafluoroethylene (ETFE)

(submitted by the website administration)

Thermoplastic
Ethylene tetrafluoroethylene (ETFE)
Property Value in metric unit Value in US unit
Density 1.74*10³ kg/m³ 108.6 lb/ft³
Modulus of elasticity 0.8 GPa 116 ksi
Flexural Modulus 1.0 GPa 145 ksi
Tensile strength 38 MPa 5510 psi
Elongation (max.) 300 % 300 %
Compressive strength 17 MPa 2470 psi
Impact strength, notched Izod >1000 J/m >18.7 ft*lb/in
Hardness 68 Shore D 68 Shore D
Thermal expansion (20 ºC) 130*10-6 ºCˉ¹ 72*10-6 in/(in* ºF)
Thermal conductivity 0.24 W/(m*K) 1.7 BTU*in/(hr*ft²*ºF)
Melting point 265 ºC 509 ºF
Maximum work temperature 155 ºC 311 ºF
Dielectric constant 2.5 - 2.5 -
Dielectric strength 25 kV/mm 625 V/mil
Electrical resistivity 1014 Ohm*m 1016 Ohm*cm
  • Good chemical resistance;
  • Good wear resistance;
  • High impact strength.

Applications: process vessels, wire and cable coating insulation, valves, pumps, packaging films, bearings.