Cast copper C80410 (Copper)
Chemical composition: Cu = 99.9% min
Property Value in metric unit Value in US unit
Density 8.94 *10³ kg/m³ 558 lb/ft³
Modulus of elasticity 117 GPa 17000 ksi
Thermal expansion (20 ºC) 16.9*10-6 ºCˉ¹ 9.4*10-6 in/(in* ºF)
Specific heat capacity 394 J/(kg*K) 0.092 BTU/(lb*ºF)
Electric resistivity 1.76*10-8 Ohm*m 1.76*10-6 Ohm*cm
Tensile strength ( centr. cast) 172 MPa 25000 psi
Yield strength (centrif. cast) 55 MPa 8000 psi
Elongation (centrifug. cast) 25 % 25 %
Hardness (centrifugal cast) 30 RF 30 RF
Liquidus temperature 1083 ºC 1981 ºF
Solidus temperature 1064 ºC 1948 ºF