Carbon-Carbon Composite (randomly oriented fibers) | ||||
Composition: carbon matrix + 40% carbon fibers | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 1.7 *10³ | kg/m³ | 106 | lb/ft³ |
---|---|---|---|---|
Flexural strength | 250 | MPa | 36300 | psi |
Fracture modulus of elasticity | 50 | GPa | 7250 | ksi |
Tensile strength | 250 | MPa | 36300 | psi |