| cg-Nicalon | ||||
| Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers (14 mkm diameter) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 2.55 *10³ | kg/m³ | 159 | lb/ft³ |
|---|---|---|---|---|
| Modulus of elasticity | 195 | GPa | 28300 | ksi |
| Tensile strength | 220 | MPa | 31900 | psi |
| Thermal expansion (20 ºC) | 3.2*10-6 | ºCˉ¹ | 1.8*10-6 | in/(in* ºF) |
| Thermal heat capacity | 630 | J/(kg*K) | 0.15 | BTU/(lb*ºF) |
| Thermal conductivity | 1.5 | W/(m*K) | 10.4 | BTU*in/(hr*ft²*ºF) |