Two component toughened epoxy adhesive
Two component toughened, thixotropic paste, high strength, high thermal resistance epoxy adhesive
Property Value in metric unit Value in US unit
Viscosity (mixed) at 77°F (25°C) 300000 cP 6.27 lbf*sec/ft²
Working strength time 2 hrs 2 hrs
Full cure time 72 hrs 72 hrs
Maximum gap 5 mm 0.2 in
Shear strength, steel-to-steel 77°F (25°C) 16 MPa 2320 psi
Peel strength, steel-to-steel 77°F (25°C) 80 N/(25mm width) 17 PIW (lbf/inch width)
Min. service temperature -40 ºC -40 ºF
Max. service temperature 120 ºC 248 ºF