Weak Base Anion Exchange Resin
Uniform Particle Size, High Capacity, Weak Base Anion Exchange Resin
Property Value in metric unit Value in US unit
Matrix Styrene-DVB, macroporous
Functional group Tertiary amine
Exchange capacity 1.3 eq/l 28.4 kgr of CaCO3/ft³
Water content 55%
Total swelling (Cl- → OH-) 20%
Mean particle size 0.53 mm 20.9 μinch
Particle density 1.04 kg/l 68.1 lb/ft³
Shipping weight 0.64 kg/l 40 lb/ft³
Maximum work temperature 100 °C 212 °F
PH range 0-7
Min. bed depth 800 mm 2.6 ft
Service flow rate 5-60 m/h 2-24 gpm/ft2
Co-current regeneration rinse 1-10 m/h 0.4-4 gpm/ft2
Counter-current regeneration rinse 5-20 m/h 2-8 gpm/ft2
Total rinse requirement 2-4 bed volumes
Regenerant NaOH (2-5%)