SubsTech     
SubsTech     

to Commercially pure and low alloyed titanium alloys
to Properties of titanium alloys

Low alloyed titanium alloy, Grade 7

(submitted by the website administration)

Low alloyed titanium, Grade 7 (Ti-0.15Pd)
Chemical composition: O=0.25% max., Fe=0.3% max., Pd=0.15%, Ti balance
Property Value in metric unit Value in US unit
Density 4.51 *10³ kg/m³ 282 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 8.6*10-6 ºCˉ¹ 4.8*10-6 in/(in* ºF)
Specific heat capacity 520 J/(kg*K) 0.124 BTU/(lb*ºF)
Thermal conductivity 20.8 W/(m*K) 144 BTU*in/(hr*ft²*ºF)
Electric resistivity 56*10-8 Ohm*m 56*10-6 Ohm*cm
Tensile strength 434 MPa 63000 psi
Yield strength 345 MPa 50000 psi
Elongation 20 % 20 %
Hardness 82 HRB 82 HRB
Melting temperature 1660 ºC 3020 ºF
Beta Transus temperature 913 ºC 1675 ºF