Alumina aerogel monolith
Chemical composition: Al2O3, derived from aluminum alkoxide, %Solids: 2%
Property Value in metric unit Value in US unit
Density 0.037 *10³ kg/m³ 2.3 lb/ft³
Internal Surface Area 376 m²/g 1.8*106 ft²/lb
Modulus of elasticity 0.00055 GPa 0.08 ksi
Thermal conductivity (100ºF/38ºC) 0.029 W/(m*K) 0.20 BTU*in/(hr*ft²*ºF)