Wrought aluminum-silicon alloy 4045
Chemical composition: Si=10.0%, Al balance
Property Value in metric unit Value in US unit
Density 2.67 *10³ kg/m³ 167 lb/ft³
Thermal expansion (20 ºC) 21.1*10-6 ºCˉ¹ 11.7*10-6 in/(in* ºF)
Thermal conductivity 171 W/(m*K) 1190 BTU*in/(hr*ft²*ºF)
Electric resistivity 3.82*10-8 Ohm*m 3.82*10-6 Ohm*cm
Liquidus temperature 599 ºC 1110 ºF
Solidus temperature 574 ºC 1065 ºF