Chemical formula: ClCH-CCl2
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 1.46*10³ kg/m³ 91.4 lb/ft³
Viscosity at 68°F (20°C) 0.58 cP 3.89*10-4 lb/ft·s
Surface tension at 68°F (20°C) 0.032 N/m 1.82*10-4 lbf/in
Vapor pressure at 68°F (20°C) 7900 Pa 1.15 psi
Boiling point 87 ºC 189 ºF
Melting Point -86 ºC -123 ºF
Autoignition temperature 410 ºC 770 ºF
Dielectric constant at 68°F (20°C) 3.27 3.27
Specific heat capacity 930 J/(kg*K) 0.222 BTU/(lb*ºF)
Latent heat of vaporization 241 kJ/kg 103.6 BTU/lb