Titanium β-alloy Ti-10V-2Fe-3Al
Chemical composition: O=0.13% max., V=10%, Fe=2%, Al=3%, Ti balance
Property Value in metric unit Value in US unit
Density 4.65*10³ kg/m³ 290 lb/ft³
Modulus of elasticity 103 GPa 15000 ksi
Thermal expansion (20 ºC) 9.7*10-6 ºCˉ¹ 5.4*10-6 in/(in* ºF)
Tensile strength 1310 MPa 190000 psi
Yield strength 1228 MPa 178000 psi
Hardness 41 HRC 41 HRC
Solution temperature 760 ºC 1400 ºF
Aging temperature 500 ºC 930 ºF
Aging time 8 hrs. 8 hrs.
Melting temperature 1649 ºC 3000 ºF
Beta Transus temperature 796 ºC 1465 ºF