Polyalphaolefin synthetic multigrade engine oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.911 *10³ kg/m³ 56.9 lb/ft³
Kinematic viscosity at 104°F (40°C) 133 cSt 133 cSt
Kinematic viscosity at 212°F (100°C) 20.7 cSt 20.7 cSt
Viscosity index 181 181
CCS viscosity at -4°F (-20°C) 4720 cP 4720 cP
Flash point 238 ºC 460 ºF
Pour Point max. -46 ºC max. -51 ºF
Sulfated ash 0.84 % 0.84 %
Neutralization No. (TBN-E) 8.4 8.4
Color 2.7 2.7