Silicate ceramic Cordierite C410

(submitted by the website administration)

Silicate ceramic Cordierite C410
Chemical composition: 3Al2O3*2SiO2, Al2O3, SiO2
Property Value in metric unit Value in US unit
Density 2.1 *10³ kg/m³ 131.1 lb/ft³
Flexural strength 60 MPa 8700 psi
Thermal expansion (20 ºC) 2.0*10-6 ºCˉ¹ 1.1*10-6 in/(in* ºF)
Thermal conductivity 2.0 W/(m*K) 13.9 BTU*in/(hr*ft²*ºF)
Dielectric constant 6 - 6 -