Silicate ceramic Alumina Porcelain C110
Chemical composition: SiO2, Al2O3
Property Value in metric unit Value in US unit
Density 2.45 *10³ kg/m³ 153.0 lb/ft³
Flexural strength 40 MPa 5800 psi
Compressive strength 450 MPa 65300 psi
Thermal expansion (20 ºC) 5.2*10-6 ºCˉ¹ 2.9*10-6 in/(in* ºF)
Thermal conductivity 1.9 W/(m*K) 13.2 BTU*in/(hr*ft²*ºF)
Dielectric constant 6 - 6 -