SubsTech     
SubsTech     
Command disabled: index

SubsTech’s sister website Smooth Sliding provides independent engineering consulting services that help you to solve engine bearing related issues: failures, material selection, geometry design and optimization of hydrodynamic conditions.

Smooth Sliding is an engineering consulting company run by Dr. Dmitri Kopeliovich:

  • World leading expert (32 years of experience) in design, technology and materials for Engine bearings in applications such as automotive, renewable energy, aviation, racing and others.
  • Founder and owner of SubsTech (Substances & Technologies) – a leading professional website on Materials Science and Engineering.
  • Author of numerous scientific and engineering publications and patents.
  • Founder and owner of Smooth Sliding.

For further information and for requesting consulting services please visit our sister website Smooth Sliding.



to Metals
to Engine bearings

Selection of engine bearing materials

Dr. Dmitri Kopeliovich

Selection of bearing material suitable for a particular engine should be based on the following engine parameters:

Stock engines, street performance and circle track racing engines may use conventional aluminum-tin-silicon bi-metal or copper based tri-metal bearings depending on the load and crankshaft materials (AlSi bi-metal – for nodular cast iron shafts, tri-metal - for forged steel shafts).

Tri-metal bearings are recommended for off-road and off-shore racing engines (typically higher loaded applications).

High strength tri-metal materials (e.g. Sputter bearings) are recommended for applications with high bearing loading where conventional tri-metal material undergoes fatigue (for example upper conrod bearings in diesel engines with direct fuel injection).

to top


Related internal links


to Metals
to Engine bearings

selection_of_engine_bearing_materials.txt · Last modified: 2023/12/13 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License