Chemical composition: carbon (C)
Property Value in metric unit Value in US unit
Density 1.55*10³ kg/m³ 96.8 lb/ft³
Modulus of elasticity 9.5 GPa 1380 ksi
Flexural strength 15 MPa 2180 psi
Compressive strength 50 MPa 7250 psi
Hardness 85 RB 10/60 85 RB 10/60
Thermal expansion (20 ºC) 3.1*10-6 ºCˉ¹ 1.7*10-6 in/(in* ºF)
Thermal conductivity 6 W/(m*K) 41.6 BTU*in/(hr*ft²*ºF)
Electric resistivity 55*10-6 Ohm*m 55*10-4 Ohm*cm


Applications: glass processing