Fluorocarbon solvent Hydrochlorofluorocarbon (Chlorodifluoromethane, Freon 22)
Chemical formula: CHClF2
Property Value in metric unit Value in US unit
Density of gas at at boiling point 4.71 kg/m³ 0.29 lb/ft³
Density of liquid at boiling point 1.413*10³ kg/m³ 88.2 lb/ft³
Viscosity at 32°F (0°C) 0.126 cP 8.47*10-5 lb/ft·s
Vapor pressure at 68°F (20°C) 908 kPa 132 psi
Boiling point -41 ºC -41 ºF
Melting point -175 ºC -284 ºF
Specific heat capacity (Cv) of gas at 86°F (30°C) 555 J/(kg*K) 0.133 BTU/(lb*ºF)
Specific heat capacity (Cp) of gas at 86°F (30°C) 659 J/(kg*K) 0.157 BTU/(lb*ºF)
Latent heat of vaporization 234 kJ/kg 101 BTU/lb