Mineral based hydraulic oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.871 *10³ kg/m³ 54.4 lb/ft³
Kinematic viscosity at 104°F (40°C) 46.3 cSt 46.3 cSt
Kinematic viscosity at 212°F (100°C) 6.94 cSt 6.94 cSt
Viscosity index 106 106
Flash point 220 ºC 428 ºF
Pour Point -30 ºC -22 ºF
Aniline Point 108 ºC 226 ºF
Color max. 2.0 max. 2.0