| High temperature compression molded carbon-graphite | ||||
| Chemical composition: carbon (C) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.8*10³ | kg/m³ | 112 | lb/ft³ |
|---|---|---|---|---|
| Flexural strength | 59 | MPa | 8555 | psi |
| Compressive strength | 152 | MPa | 22040 | psi |
| Hardness (Shore) | 80 | HS | 80 | HS |
| Thermal expansion (20 ºC) | 2*10-6 | ºCˉ¹ | 1.1*10-6 | in/(in* ºF) |
| Thermal conductivity | 69 | W/(m*K) | 478 | BTU*in/(hr*ft²*ºF) |
| Max. service temperature in air | 649 | °C | 1200 | ºF |
Applications: high temperature, high strength.