| Extruded carbon | ||||
| Chemical composition: petroleum coke based baked carbon (C), ash 0.2% | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.62*10³ | kg/m³ | 101 | lb/ft³ | 
|---|---|---|---|---|
| Maximum grain size | 760 | μm | 30 | microinch | 
| Flexural strength | 15.9 | MPa | 2300 | psi | 
| Tensile strength | 11.7 | MPa | 1700 | psi | 
| Compressive strength | 38.5 | MPa | 5585 | psi | 
| Thermal conductivity | 10 | W/(m*K) | 69.3 | BTU*in/(hr*ft²*ºF) | 
| Electric resistivity WG (with grain) | 42*10-6 | Ohm*m | 42*10-4 | Ohm*cm | 
| Electric resistivity AG (against grain) | 50*10-6 | Ohm*m | 50*10-4 | Ohm*cm | 
 Applications: anodes for electroplating, low thermal conductivity applications.
 http://www.carbonandgraphite.org/
 http://virtual-museum.soils.wisc.edu/graphite/content.html
 http://www.uwm.edu/Course/422-100/Mineral_Rocks/graphite.data.html
 http://www.public.asu.edu/~jpbirk/3dstruct/Graphite.htm
 http://invsee.asu.edu/nmodules/Carbonmod/bonding.html
 http://www.gc.maricopa.edu/earthsci/imagearchive/graphite.htm
 http://www-ferp.ucsd.edu/LIB/PROPS/PANOS/c.html
 http://www.phy.mtu.edu/faculty/info/jaszczak/graphiteover.html
 http://encyclopedia.jrank.org/GOA_GRA/GRAPHITE.html
 http://www.minerals.net/mineral/elements/graphite/graphite.html