Carbon Fiber Reinforced Polymer (CFRP)
Composition: 50% carbon fibers in epoxy matrix
Property Value in metric unit Value in US unit
Tensile strength (LW) 1448 MPa 210000 psi
Tensile strength (CW) 52 MPa 7500 psi
Compressive strength (LW) 600 MPa 87000 psi
Compressive strength (CW) 206 MPa 30000 psi
Shear strength 93 MPa 13500 psi

LW- Lengthwise direction, CW- Crosswise direction