Compressor oil ISO 32

(submitted by the website administration)

Compressor oil ISO 32
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.861 *10³ kg/m³ 53.7 lb/ft³
Kinematic viscosity at 104°F (40°C) 32.7 cSt 32.7 cSt
Kinematic viscosity at 212°F (100°C) 5.6 cSt 5.6 cSt
Viscosity index 109 109
Flash point 226 ºC 439 ºF
Pour Point -15 ºC 5 ºF
Color 0.5 0.5
NOACK volatility (weigh loss) 15.04 % 15.04 %

Applications: screw compressors.