Compression molded carbon
Chemical composition: carbon (C), ash 0.3%
Property Value in metric unit Value in US unit
Density 1.65*10³ kg/m³ 103 lb/ft³
Porosity 18 % 18 %
Maximum grain size 760 μm 30 microinch
Modulus of elasticity 6.2 GPa 900 ksi
Flexural strength 9.7 MPa 1400 psi
Compressive strength 26.2 MPa 3800 psi
Thermal conductivity 25 W/(m*K) 173 BTU*in/(hr*ft²*ºF)
Electric resistivity 23*10-6 Ohm*m 23*10-4 Ohm*cm


Applications: furnace parts, fluidized bed reactors, chemical equipment