Circulating rust protection oil ISO 68 | ||||
Mineral based oil with volatile corrosion inhibitor | ||||
Property | Value in metric unit | Value in US unit | ||
Density at 60°F (15.6°C) | 0.866 *10³ | kg/m³ | 54.1 | lb/ft³ |
---|---|---|---|---|
Kinematic viscosity at 104°F (40°C) | 68.3 | cSt | 68.3 | cSt |
Kinematic viscosity at 212°F (100°C) | 8.6 | cSt | 8.6 | cSt |
Viscosity index | 107 | 107 | ||
Pour Point | -27 | ºC | -17 | ºF |
Copper strip corrosion test at 212°F (100°C) for 3hrs. | 1 | 1 | ||
Color | 1.5 | 1.5 |
Applications: circulating and lubricating systems, in which steel parts above the oil level should be protected (oil storage tanks, circulating reservoirs).