Cast copper alloy C96400 (70-30 Copper-Nickel) | ||||
Chemical composition: Ni=30%, Fe=0.9%, Nb=1.0%, Cu=balance | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 8.94 *10³ | kg/m³ | 558 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 145 | GPa | 21000 | ksi |
Thermal expansion (20 ºC) | 16.2*10-6 | ºCˉ¹ | 9.0*10-6 | in/(in* ºF) |
Specific heat capacity | 377 | J/(kg*K) | 0.090 | BTU/(lb*ºF) |
Thermal conductivity | 28.5 | W/(m*K) | 197 | BTU*in/(hr*ft²*ºF) |
Electric resistivity | 35.7*10-8 | Ohm*m | 35.7*10-6 | Ohm*cm |
Tensile strength (sand cast) | 469 | MPa | 68000 | psi |
Yield strength (sand cast) | 255 | MPa | 37000 | psi |
Elongation (sand cast) | 28 | % | 28 | % |
Fatigue strength (sand cast) | 124 | MPa | 18000 | psi |
Hardness (sand cast) | 140 | HB(3000) | 140 | HB(3000) |
Liquidus temperature | 1238 | ºC | 2260 | ºF |
Solidus temperature | 1117 | ºC | 2140 | ºF |